Curl after laminating
Medium severitySymptoms
One-side laminated sheet curving toward the film
Probable causes
- High film tension
- low paper grammage
- moisture difference between sides
The Print Guy · 2026-10-05
Other problems in this category
Lamination · TPG-160
Scratched film or hard particles
Scratches or hard dots visible under the laminate
Lamination · TPG-161
Silvering
Uniform silvery micro-dots of air, mostly over dark inks
Lamination · TPG-157
Bubbles under the film
Visible air blisters after laminating
Lamination · TPG-158
Delamination at edges and folds
Film separating from the print over time or at folding