New blanket repelling ink
Low severitySymptoms
First sheets come out washed-out after a blanket change
Probable causes
- Factory protective layer (talc/agents) not removed
The Print Guy · 2026-10-05
Other problems in this category
Blankets · TPG-083
Blanket edge marks on the print
Lines or shadows at the format edges
Blankets · TPG-078
Glazed blanket
Smooth shiny surface; poor transfer, washed-out solids, slurring
Blankets · TPG-079
Blanket swelling
Swollen area printing with more pressure; local gain, registration affected
Blankets · TPG-080
Height loss / fatigue-flattened blanket
Overall insufficient pressure; weak image despite correct packing
Blankets · TPG-081
Blanket delamination
Blister or bubble under the surface; locally distorted image
Blankets · TPG-082
Wrong blanket tension
Loose: doubling, wrinkles. Overtensioned: crushed carcass, short life