Binding (hotmelt/PUR) problems: causes and fixes
8 Binding (hotmelt/PUR) problems in offset and finishing: symptoms, causes and how to spot them. Step-by-step fixes with your account.
Binding (hotmelt/PUR) · TPG-229
Pages pulling out (low pull test)
Loose pages when opening the book; pull test < 6 N/cm
Binding (hotmelt/PUR) · TPG-230
Spine cracking open (cold crack)
Spine snaps and pages release, especially in cold conditions
Binding (hotmelt/PUR) · TPG-231
Glue not wetting the spine (voids)
Spine zones without glue; locally loose pages
Binding (hotmelt/PUR) · TPG-235
Cover detaching from the block
Cover separating from the spine or side guards
Binding (hotmelt/PUR) · TPG-232
Glue squeeze-out
Glue visible at the cover joint or between pages
Binding (hotmelt/PUR) · TPG-233
PUR not curing / soft spine days later
Spine still soft or smelly after 48 h
Binding (hotmelt/PUR) · TPG-234
Spine waving
Wavy spine or book that won't close flat
Binding (hotmelt/PUR) · TPG-236
Saddle stitching crooked or off-center
Staples off the spine; misaligned signatures