High severitySymptoms
Sheets curling toward the PE side at the feeder or after printing; registration and feeding impossible
Probable causes
- Asymmetric build (fiber absorbs moisture, PE doesn't): any humidity or heat change bends the sheet
- dampening water absorbed only by the fiber side
- IR dryer heat
The Print Guy · 2026-10-05
Other problems in this category
Polyboard/Corona · TPG-119
Ink won't adhere on polyboard (PE)
Ink scratches off with a nail or lifts with tape; image 'floating' on the surface
Polyboard/Corona · TPG-120
Corona treatment decays over time
Stock that printed fine weeks ago now rejects ink; dynes lower than the supplier declared
Polyboard/Corona · TPG-122
Uneven corona treatment (bands or untreated zones)
Good adhesion in parts of the sheet, poor in others; visible bands with test ink
Polyboard/Corona · TPG-123
Slow or no ink drying on polyboard
Ink wet for hours or days; massive set-off; job can't be finished
Polyboard/Corona · TPG-124
Set-off and blocking in the pile with polyboard
Sheets stuck together; ink transferred to the PE face of the next sheet
Polyboard/Corona · TPG-128
Blocking of fiber side against PE side in the pile
Ink printed on the fiber side transfers to the PE side of the sheet above; stuck sheets